Methacrylate Structural Adhesives
September 24, 2001
ITW PLEXUS
This company has obtained American Bureau of Shipping (ABS) certification for four of its methacrylate structural adhesives: Plexus MA555, MA556, MA550 and MA425. This prestigious certification is awarded to products that demonstrate consistently high quality and performance in ABS-Class marine vessels. These two-part methacrylate adhesives are designed for structural bonding of thermoplastic, metal and composite assemblies. They require virtually no surface preparation and provide excellent fatigue endurance, impact resistance and toughness. Circle No. 115