This company has announced
the availability of CoatOSil
TM MP 200 silane and
CoatOSil DSA 6 friction modifier.
CoatOSil MP 200 silane is
the latest addition to Momentive’s CoatOSil line of silanes for protective
coatings. CoatOSil MP 200 silane has
broad-based utility and can be considered for use in both solvent and
water-based formulations. It can help enhance corrosion resistance and promote
the adhesion of epoxy paint by creating a covalent bond linking the paint to a
metal surface. In addition to acting as a useful crosslinker in many water- and
solvent-based systems, CoatOSil MP 200 silane offers reduced VOC generation
when compared to traditional epoxy silanes.
CoatOSil DSA 6 friction
modifier is a silicone-based resin that can be used as an additive to coatings
for the improvement of performance as well as provision of a variety of slip
and soft-touch characteristics. In addition to providing a marked reduction in
coefficient of friction when formulated into a properly designed coating
system, CoatOSil DSA 6 friction modifier has a lower specific gravity than
conventional inorganic fine powders, while still offering excellent heat and
chemical resistance.
For more information, visit
www.momentive.com.