Moore Enviro-Chemical
April 17, 2000
Moore Enviro-Chemical has produced an environmentally safe chemistry that completely dissolves fully cured silicone sealants and related products.
Moore Enviro-Chemical, Inc. (MEC), Camarillo, Calif., has produced an environmentally safe chemistry that completely dissolves fully cured silicone sealants and related products. Cleaning times are reduced from days to hours or minutes. The product is a unique blend of non-toxic materials designed to dissolve silicone-based materials from a range of manufacturers. The product is non-flammable, does not contain chlorinated or other toxic substances, and is safe for metallics and other sensitive substrates.