Adhesives Magazine

National Starch: National Adhesives' Pamphlet Listing Performace Test Results

September 17, 2003
A new pamphlet describes performance results of six tests that can help window manufacturers evaluate the effectiveness of an instant strength, curable, hot melt sealant. Three sets of curves also graphically show various relationships. These include stress vs. strain for the Purfect Glaze sealant compared with silicone; lap shear strength vs. time for this sealant compared with silicone and tape sealants; and temperature vs. time during a six-hour, accelerated weather cycle for this sealant.

For a copy, call 800-797-4992 or fax 609-409-5699.

http://www.nationalstarch.com