Underwriters Laboratories Inc. has approved North Sea Resins' (NSR) NSR150 and NSR250 products per ANSI/NSF Standard 61, Drinking Water Systems Components - Health Effects. As part of NSR's Rapid Repair Kits, NSR150 and NSR250 are the only Cure-on-Command resins that are NSF Standard 61 approved. Pipes, tanks and equipment that must be maintained/repaired in compliance with drinking water standards can be repaired either when wet or dry by taking advantage of 30 second cure times that are uniquely a part of the North Sea Resins Rapid Repair Kit. NSR150 resin has been optimized for repairing holes and cracks that occur in PVD, CPVD, ABS, polyethylene and other non-metal materials. NSR250 resin has been optimized for repairing holes and cracks that occur in copper, brass, steel, cast iron, black pipe, aluminum, and other metal substrates.