Optically Clear Adhesives
ADHESIVES RESEARCH, INC.
The ARclear line of optically clear transfer adhesives is a diverse product line that includes permanent, strippable and silicone adhesives for the assembly of flat-panel displays, flat-screen CRTs, large and small LCDs, and touch screens. The adhesives are non-birefringent, with low haze (<1%), high clarity (>97%) and high light transmission (>95%). They offer long-term durability and are environmentally robust to resist temperature extremes, humidity and UV light. Circle No. 143