Permabond 2011 adhesive is designed to bond plastics, rubber, ceramics and metal. It is best suited for applications that require a high viscosity for ease of dispensing or to facilitate gap filling. Thin bond lines will cure almost instantly. In larger gaps, the cure speed will be reduced to allow for proper positioning prior to cure. This high viscosity adhesive will not run or sag, even on vertical surfaces. Cyanoacrylates are single-component adhesives that cure by reacting with small traces of moisture on the surface of the substrates being bonded. Permabond offers a complete line of cyanoacrylates that vary in adhesion to different substrates, viscosity, temperature resistance, color, gap-filling capability, cure speed and compatibility.
For more information, visit http://www.permabond.com or call (800) 640-7599.