Plastic Antimicrobial
AVECIA BIOCIDES
This company has announced U.S. EPA registration for its new Vanquish™ 100 plastics antimicrobial — the first new biocidal active ingredient to be registered as a preservative for plastics in the United States in the last five years. Based on a dual-purpose preservative and effects molecule, this product features broad spectrum activity and incorporates the active nBBIT (N-Butyl-1, 2-benzisothiazolin-3-one). In preservation mode, Vanquish100 prevents deterioration of plastics while its effects capabilities prevent bacterial and fungal surface growth. Applications include polypropylene, polyethylene, PVC, silicones and polyurethanes.
For more information, call (800) 523-7391.