Polysciences, Inc., a leading manufacturer of specialty monomers/polymers for electronics, has introduced LoSTRESS™ SF54GB, an environmentally green version of its popular LoSTRESS liquid encapsulant. LoSTRESS SF54GB maintains all of the excellent physical properties of previous product versions, but does not contain brominated flame-retardants, antimony oxides, or other banned materials. In addition, this green version shows significantly improved long-term aging performance, allowing for higher reliability and increased thermal shock resistance.
For more information, visit http://www.PSIinfo.com/90.