Adhesives Magazine

Potting Compounds

September 1, 2001
Dymax Corp.
Potting Compounds
DYMAX CORP.
This company's new potting compounds provide an instant UV-curing feature with the ability to cure at room temperature to depths of an inch or more and in areas under components where the light does not reach. Designated 960A/B and 961A/B, the new products are designed for ease of application through typical disposable-tip static-mix dispensers. Following dispensing, exposure to long-wave UV light cures the products to a depth of 1┬┐inch in 20 seconds or less. The remaining liquid resin gels in seven to 20 minutes. Full cure is achieved in 24 hours at room temperature. Circle No. 147