PBWMF-4 white masking film is a 3-mil polyolefin film coated with a removable acrylic adhesive that can prevent damage to glass, auto trim, clear-coated aluminum, and other highly polished finishes. The adhesive does not build over time and can remove cleanly from most surfaces up to one year after application. The adhesive delivers a cling-like, low initial grab, which allows for clean repositioning to find the perfect fit while providing environmental resistance (-20° to 150°F) and aging properties.