PROGRESSIVE EPOXY POLYMERS INC.: Epoxy Patch

November 19, 2008


Epoxy Mortar PatchTM is a two-component, 100%-solids pourable epoxy. This product is recommended for repairing defects in concrete or masonry products by mixing with sand to form an “epoxy mortar.” The product can be used on wet or submerged surfaces.

With the addition of approximately 15 pounds of sand added to the 1.5-gal epoxy kit, approximately 2.5 gallons (about 575 cubic inches) of repair epoxy is generated. Applications for this product include airport runway repair, spalling factory floor repair, and crack and pothole repair.

For more information, visit www.epoxyproducts.com.