This company now offers a water-based
epoxy primer called Water Prime
TM.
Progressive Epoxy Polymers
Inc., an Internet supplier of epoxy resins/coatings, urethanes, fillers and
thickeners for commercial, residential, and marine use, now offers a water-based
epoxy primer called Water Prime
TM.
Water Prime is a gray-pigmented,
water-based (contains some solvent) epoxy with an easy 4:1mix ratio by volume.
Advantages of Water Prime
include easy water clean-up, less dripping and sagging than solvent-free or
solvent-based epoxies, and extremely long pot life.
Due to VOC restrictions, Water
Prime cannot be sold in all parts of the country.
This product is sold in
40-ounce kits for $28 and one-gallon kits for $80.
For more information, visit
www.epoxyproducts.com/datamsds.html.