April 30, 2002
NATIONAL STARCH & CHEMICAL CO.

DURO-TAK(r) 80-115A is a modified, acrylic-solution, pressure sensitive adhesive designed for adhesion to low-energy surfaces. This one-part, self-crosslinking adhesive adheres well to polyolefin substrates and plastics, making it well suited for film and foil tapes, and transfer-films and tapes. Test results show that bond strength continues after immersion in water for one week at room temperature. Bond strength also remains after exposure to mild acids, mild bases and many other chemicals. Circle No. 122