This company has introduced two new specialty monomers: GENOMER 1119 and GENOMER 1121M. The products are acrylic acid ester and are recommended for radically curable inks, coatings, and adhesives. GENOMER 1119 is 4-tert-butylcyclohexyl acrylate and GENOMER 1121M is isobornyl methacrylate.
GENOMER 1119 features high flexibility, medium-high hardness, low shrinkage and good adhesion. 1121M offers low shrinkage, good adhesion, and low yellowing. In addition, it is hydrophobic and reportedly good for heat and water resistance