September 27, 2000
Reichhold has introduced ELVACE® 737, a high-solids, polyvinyl-alcohol-stabilized vinyl acetate-ethylene copolymer emulsion.
Reichhold, Research Triangle Park, N.C., has introduced ELVACE® 737, a high-solids, polyvinyl-alcohol-stabilized vinyl acetate-ethylene copolymer emulsion. The product is designed as a base for special-purpose or general adhesives. It features excellent wet tack; fast setting speed; excellent machining; and good adhesion to packaging film and foil, and PVC film.