This company has added an optically clear, thin gauge polyester release liner to its Clearsil release film product line. This liner offers a total haze of less than 2% and is available on 1-, 1.5- and 2-mil PET with easy, tight or differential silicone release coatings. It is intended for use in applications requiring clear, clean liners such as optically clear PSA tapes, graphic arts, overlaminating films and electronics.