Resinall Corp. recently announced its plans to construct a hydrogenated hydrocarbon resin unit at its Hattiesburg, MS, manufacturing site. The new unit will produce low-molecular-weight thermoplastic resins that offer elastomer and plastic compatibility. The facility will use a modular design to facilitate increases in capacity and keep pace with market growth and product demand.
Phase I is targeted for completion and startup in 2012, and will be capable of producing multiple resin grades. Products will be available in both solid and molten form.