The Hycasyl™ family of hydrolysis stabilizers can be used to prolong the performance life of many types of polyurethane adhesives, particularly in the flexible packaging, electrical, electronics and shoe sole markets. The new stabilizers are especially useful for higher temperature and moisture applications, where they have demonstrated up to 13 times longer adhesive life and up to twice the adhesive strength of unstabilized adhesives in lab tests.