RoSeal™ acrylic adhesives were specially developed for use by tape manufacturers in the production of their high-quality carton-sealing tapes. Performance attributes include a broad temperature tolerance, excellent moisture resistance, nonyellowing appearance, good printability and long-lasting adhesion. Carton-sealing tapes backed with RoSeal apply smoothly, evenly and with control.