Sartomer Co. has announced the introduction of a line of
acrylate oligomers for photovoltaic (PV) applications. Based on polybutadiene
or hydrogenated polybutadiene, Sartomer’s oligomers are ideally suited as
formulation ingredients for PV barrier coatings, sealants, adhesives,
dielectrics and encapsulents. Sartomer oligomers offer good oxygen, moisture
and chemical resistance, and will yield films that are flexible and have low
T
g. Hydrogenated products offer the additional benefit
of color and physical property stability against light and environmental
degradation.
CN307, CN308, CN309 and CN9014 oligomers are now commercially
available. Additional products will be released soon.