Scapa has introduced Duofoam S3632W, a double-coated white polyethylene foam tape specifically designed for window manufacturing applications. The product is A.A.M.A. Certified 810.1-92 for window glazing. Double-coated with a solvent-based acrylic pressure sensitive adhesive and supplied on a silicone-coated draft release liner, this product offers high load end bearing ability, uniform unwind, and easy die cutting. Duofoam S3632W will perform over a wide temperature range and offers excellent long-term aging and environmental durability. The product is highly conformable to irregular surfaces and maintains its seal on high movement joints. This tape offers good thermal insulation properties.
For more information, visit http://www.scapaindustrial.com .