SCAPA: Medical Foam Adhesive

January 13, 2005
Scapa Medical now offers Bioflex Rx232V-60, a single-coated, medical-grade polyethylene foam adhesive for use in medical device assembly or direct skin contact applications. Rx232V-60 consists of a soft white polyethylene foam, single-coated with a medical grade acrylic pressure-sensitive adhesive that carries a Drug Master File Number. The film is supplied on a 60# white kraft release liner. The acrylic adhesive offers excellent quick stick and good adhesion, yet removes cleanly from skin without causing trauma. The product is used in medical device manufacturing, ECG electrode fabrication, and for specialty bandage production.