Scapa Medical now offers Medifix 6016/868, a medical grade pressure sensitive adhesive (PSA) film for direct skin applications including wound and IV care, consumer dressings, and cutaneous attachment of medical devices. Medifix 6016/868 consists of a soft, conformable 0.4 mm transparent polyurethane film coated on one side with a medical grade acrylic adhesive. The product is supplied on an 80-gsm white glassine release liner and can be provided with or without a polyethylene delivery film.
For more information, visit http://www.scapamedical.com or call (800) 653-5312.