Scapa Medical offers Bioflex 235, a breathable, medical-grade thermoplastic co-polyester extruded film for wound dressing and surgical drape and gown fabrication. The film provides good barrier properties and can be laminated to a variety of substrates. The product is supplied on a casting sheet and is available in thicknesses of 1 to 3 mils.