Scapa North America offers a heat-reactive, thermosetting adhesive film called ThermoFilm H153U for bonding, laminating, mounting and gasketing applications. An unsupported nitrile phenolic transfer film, it provides high bond strength that is considered to be structural for many applications. Once cured, this product offers strong resistance to solvents, plasticizers and heat. Its relatively low bonding temperature allows this film to be used on temperature-sensitive substrates. The transfer film is supplied on a 60# kraft release liner.
For more information, call 800-653-5316.
http://www.scapana.com