Adhesives Magazine

Self-Lubricating Elastomer by GE Silicones

March 4, 2003
Self-Lubricating Elastomer by GE Silicones

FSL7586/40 liquid self-lubricating fluorosilicone elastomer is designed for use in gasketing and sealing applications both under the hood and on the automotive power train. The product can provide improved resistance to both lubricants and fuels, and is characterized by a low compression set without need for post-cure operations. It provides reduced insertion force for either manual or automated manufacturing processes. High curing speed and easy de-molding permit fully automated production of large numbers of articles in short cycle times.