DOCK RESINS CORP.

Sold under the DORESCO(r) trade name, seven resins have been developed for a variety of pressure sensitive tape and label applications. Key products include AA60-8, a thermoplastic acrylic resin supplied in a 45% nonvolatile solution; AA53-16 acrylic resin, a 40%-solids solution containing both hydroxyl and carboxyl functionalities; and AA84-1 high-quality, self-crosslinking acrylic adhesive in a 36% nonvolatile solution. Circle No. 104