The MAXIMA™ ML- 3500C UV lamp can reduce the cure time for adhesives, coatings, inks, epoxies, resins, printed circuit boards, plastics and other materials. The lamp produces a nominal steady-state UV-A intensity of 75,000 µW/cm² at 6 in. (15 cm) for high-speed curing and increased production. The lamp has an ergonomic design and stay-cool hand gripthat allow long periods of use without stress or fatigue. Its bulb/reflector assembly is a single, integral unit with no exposed circuitry.