This company’s STATOMIX
® line of static mixers includes a variety of plastic
disposable mixers used with meter-mix and dispense equipment that provides a
low-cost solution for two-component mixing. The mixer element is molded from
polyacetal to withstand the high pressures generated by meter-mix machines. The
STATOMIX line also includes cartridge mixers for use with handheld dispensing
equipment.
Sulzer Mixpac USA Inc. (formerly ConProtec Inc.) is an
engineering-based company focused on developing the MIXPAC
® SYSTEM for the handheld
dispensing of two-component adhesives and sealants, as well as the complete
line of STATOMIX Motionless Mixers.
For more information, visit
www.sulzermixpacusa.com.