tesa tape, inc., an affiliate of tesa SE, has introduced two new specialty products with silicone adhesive systems designed for temporary masking applications. tesa® 50650 and tesa® 50600 join the company’s masking product line, which includes general-purpose and highly specialized masking tapes.
These tapes were developed with specialty masking and holding applications in mind. Constructed of a durable polyester film backing coated with a distinctive silicone adhesive, tesa 50650 and 50600 are designed to perform well in harsh and demanding conditions, including withstanding temperatures of up to 428°F for up to 30 minutes. The resilient polyester backing is resistant to abrasions, as well as to chemical and thermal elements, and the tapes’ crisp edges produce sharp paint lines.
More information:
www.tesatape.com.