Tra-Con: Fiber Optic Connector Adhesive

May 4, 2000
TRA-BOND F131 is a clear, low-viscosity material specifically formulated for terminating all types of fiber optic connectors. This two-part material is easy to mix and cure at room temperature, although at 65ºC a cure time of 15 minutes can be achieved. This high-strength, non-positioning material exhibits a glass transition temperature of 95ºC. It is suggested for bonding optical lenses, mirrors and other components, and has superior bond strength to glass, plastics and metals.