Tra-Con: Room-Temperature-Curing Adhesive
April 27, 2000
TRA-DUCT 2902 is an electrically conductive, silver-filled epoxy adhesive recommended for electronic bonding and sealing applications that require a combination of excellent mechanical and electrical properties. This two-part epoxy adhesive develops durable electrically and thermally conducting bonds and coatings between many materials, such as ceramics, metals, plastic laminates and glass. It can be cured over a range of temperatures, including room temperature. It is an excellent candidate for solder replacement where heat-sensitive components are used.