Tridak: cartridge-filling machine

August 29, 2000
This company’s new filling machine, the FILLA, overcomes the problem of achieving consistent, level, void-free fills, as well as time-consuming cleanup procedures. This bench-top cartridge/syringe dispense system automatically fills to accurate, repeatable, preset levels. Although it was designed to handle medium- to heavy-viscosity materials, it has proven to be equally efficient with many low-viscosity materials.