Nashua Tape Products introduces a new duct tape that can take the heat of outdoor repair projects. Tyco has made its Nashua brand High Heat Duct Tape - an industrial product used in some of the world's most heat-intensive environments - available to consumers. The tape is ideal for temporary outdoor use in locations where hot weather and sun are issues. Manufactured in Franklin, KY, by Tyco Adhesives, Nashua High Heat Duct Tape is produced with an adhesive formulated to retain its holding power in temperatures up to 200 degrees F. With an 80 oz./in. adhesion rating, it even adheres well to steel. The 10-mil-thick tape tears easily and features a tan color that does not absorb heat. Nashua High Heat Duct Tape is available at hardware and home improvement stores.
For more information, visit http://www.tycoadhesives.com. or call (800) 248-7659.