Tyco has announced the introduction of a new line of foil tapes specifically formulated to help heating ventilation and air conditioning (HVAC) systems withstand extreme temperatures. Available under Tyco's Nashua and Polyken brands, the 330 Extreme Weather Foil Tape is an industrial formulation ideal for securing joints and seams in duct work for HVAC systems. Developed and manufactured by Tyco Adhesives, a business unit of Tyco Plastics and Adhesives, the 330 Extreme Weather Foil Tape offers an aggressive, high-performance acrylic adhesive system that maintains superior adhesion in temperatures ranging from -35 degrees F to 260 degrees F. Featuring a "quick stick" formulation, the 330 Extreme Weather Foil Tape has a conformable foil backing that will match most laminated duct work.
For more information, visit http://www.tycoadhesives.com, call (508) 918-1682 or e-mail Paul Brodowski at BrodowskiP@tycoadhesives.com.