MERECO TECHNOLOGIES GROUP COMPANIES

MRC 03-1340 is part of a new class of Mereco UV/visible light/heat-curing UV adhesives designed to create very-high-strength bonds between glass, steel, stainless steel, aluminum, ceramic and some plastics. Bonds are optically clear and very resistant to moisture and heat. The product is available in several viscosities.