Adhesives Magazine

UV-Light-Resistant Adhesive by National Starch and Chemical Co.

March 4, 2003
UV-Light-Resistant Adhesive by National Starch and Chemical Co.



The DURO-TAK 80-109A family of solvented adhesives resists the effects of ultraviolet (UV) light and high temperatures. This family of adhesives retains clarity when less-advanced adhesives would become yellow. For many applications when there is exposure to sunlight, ranging from sunscreen containers to windows, these permanent adhesives remain clear.