UV Process Supply's patent-pending, 375nm CON-TROL-CURE UV-LED CURE-ALL is an instant-on/instant-off curing system that requires no mechanical shutters, emits no heat and has a consistent output lamp life of over 50,000 hours. The unique design allows it to be sized exactly to the end user's specifications. Extremely low-energy consumption, combined with the absence of costly replacement parts, greatly lowers the long-term operating cost for this innovative system. The UV-LED CURE-ALL is available in 5 standard configurations, including 3 linear arrays (375nm, 395nm and 415nm) and 2 spot units (390nm and 415nm). All system wavelengths, except for the new 375nm, are considered in the safe UV range for both eye and skin exposure.
For more information, visit http://www.uvprocess.com or call (800) 621-1296.