VENTURE TAPE CORP.: UV-Resistant Facing
June 1, 2008
Venture Tape Corp. has introduced
VentureWrap 1555W/U, a white, zero-perm, UV-resistant facing that can be used
as a sealant inside ductwork or as a low-temperature vapor barrier on freezer
walls where permeability is a concern. It is also used as a zero-perm jacketing
on all types of pipe insulation. Insulation and refrigeration contractors will
favor this product as an alternative to many other vapor retarders.
1555W/U is a three-ply laminate
constructed of 1 mil aluminum foil in between a layer of 0.5 mil polyester film
and a white polypropylene outer layer. It can also be used over other types of
pipe insulation, including foam glass, urethane, Styrofoam or fiberglass, and
can be applied with spray glue, double-sided tape or with Venture Tape 1555CW-W
tape.
VentureWrap is ASTM E-84 listed and
cuts and fabricates easily. Its temperature resistance ranges from minus 40