Water-Based Primer
September 24, 2001
ADM TRONICS UNLIMITED, INC.
This company offers Polaqua 103, a versatile, water-based primer/adhesive product for extrusions and laminations. When used in the converting and ink industries, compatible combinations of the product with LDPE-Surlyn-printing inks to accepting substrates include polyester, polypropylene, nylon, vinyl, PVDC, Aclar, aluminum foil, polycarbonate, paper and board, and cellophane. The product exhibits excellent grease- and oil-resistant bond strengths using only minute application levels. Circle No. 100