ROLLPRINT PACKAGING PRODUCTS INC.: Solvent-Free Overwrap

Rollprint Packaging Products, Inc. recently launched Triad, a new high-barrier, solvent-free overwrap developed using the company’s proprietary metallocene-based sealant chemistry. The sealant layer bonds to foil without the use of solvent or water-based materials.

Triad is an extrusion-coated lamination of polyester, aluminum foil and metallocene that has been engineered to provide strong hermetic weld seal in high-speed, chemically-sensitive pharmaceutical applications. Equally important, the performance benefits can be achieved at a cost-competitive price.

The water-based bonding agents designed to avoid the use of solvents typically do not hold up well with products that contain water or require high bond. Rollprint’s Triad addresses all those issues by using chemically-clean bonding agents and a sealant layer to offer high moisture and oxygen barrier at sealing speeds of more than 100 linear feet per minute.

For more information, visit www.rollprint.com.

Did you enjoy this article? Click here to subscribe to Adhesives & Sealants Industry Magazine.

You must login or register in order to post a comment.

Multimedia

Videos

Podcasts

Environmentally Friendly Manufacturing

Edward Gotch, president of Emerald Kalama Chemical, talks about embracing sustainability with Susan Sutton, editor-in-chief.

More Podcasts

THE MAGAZINE

Adhesives & Sealants Industry Magazine

ASI June 2013 cover

2013 June

The 2013 June Adhesives and Sealants Industry Magazine includes articles about Nordson EFD and UV curing with lasers, as well as a case study on progressive cavity pumps. Check it out today!

Table Of Contents Subscribe

THE ADHESIVES STORE

handbook-sealant-tech.gif
Handbook of Sealant Technology

The Handbook of Sealant Technology provides an in-depth examination of sealants, reviewing their historical developments and fundamentals, adhesion theories and properties, and today’s wide range of applications.

More Products

asi1211p_Cover-DE.gifASI's Buyers' Guide

Annual purchasing resource for equipment used in the manufacture/formulation of adhesives, sealants, pressure sensitives, tapes and labels and for application of finished adhesives. 

Clear Seas Research

With access to over one million professionals and more than 60 industry-specific publications, Clear Seas Research offers relevant insights from those who know your industry best. Let us customize a market research solution that exceeds your marketing goals.

STAY CONNECTED

facebook_40px twitter_40  youtube_40pxlinkedin_40