Emerson & Cuming D 125 F 5 is a one-component epoxy, surface-mount adhesive designed specifically for stencil printing very large components. The adhesive works well with all standard SMT stencil printers and has low moisture absorption, which translates to outstanding stencil work life. The adhesive, which is supplied in fluorescent-yellow paste form, cures in 2.5 minutes at 120 deg C. Circle No. 114