TRA-CON Offers Thermally Conductive Epoxy Adhesive

TRA-BOND 2153 is a low CTE, thermally conductive epoxy adhesive now available from TRA-CON. This product works well on staking transistors, diodes, resistors, integrated circuits and other components to circuit boards. TRA-BOND 2153 readily bonds to most metals, silica, ceramics, glass, plastic and a plethora of other materials. It has excellent electrical insulation capabilities while providing thermal transfer between substrates. The low coefficient of thermal expansion (CTE) makes TRA-BOND 2153 a good match for most materials over a wide temperature range. TRA-BOND 2153 shows exceptional resistance to salt solutions, mild acids, alkalis and other harsh chemicals.

For more information, visit http://www.tra-con.com or call (800) TRA-CON1.

Did you enjoy this article? Click here to subscribe to Adhesives & Sealants Industry Magazine.

You must login or register in order to post a comment.

Multimedia

Videos

Podcasts

Environmentally Friendly Manufacturing

Edward Gotch, president of Emerald Kalama Chemical, talks about embracing sustainability with Susan Sutton, editor-in-chief.

More Podcasts

THE MAGAZINE

Adhesives & Sealants Industry Magazine

ASI May 2013 cover 100x133

2013 May

The 2013 May Adhesives and Sealants Industry Magazine includes articles about PPG and Bostik, as well as a Q&A about polyurethane. Check it out today!

Table Of Contents Subscribe

THE ADHESIVES STORE

handbook-sealant-tech.gif
Handbook of Sealant Technology

The Handbook of Sealant Technology provides an in-depth examination of sealants, reviewing their historical developments and fundamentals, adhesion theories and properties, and today’s wide range of applications.

More Products

asi1211p_Cover-DE.gifASI's Buyers' Guide

Annual purchasing resource for equipment used in the manufacture/formulation of adhesives, sealants, pressure sensitives, tapes and labels and for application of finished adhesives. 

Clear Seas Research

With access to over one million professionals and more than 60 industry-specific publications, Clear Seas Research offers relevant insights from those who know your industry best. Let us customize a market research solution that exceeds your marketing goals.

STAY CONNECTED

facebook_40px twitter_40  youtube_40pxlinkedin_40