This company has developed 7333-74 adhesive, a new transfer adhesive specifically designed for superior foam bonding. This unsupported adhesive offers excellent bonding characteristics to a broad spectrum of foam substrates including challenging products. Additional features include superior elevated temperature performance; an easy-release, 74-pound liner that enhances die cutting; high peel strength; high shear resistance; and a biostatic additive that inhibits microbial growth.