Arclad(r) 9032 is a 1-mil, electrically conductive, acrylic pressure sensitive transfer adhesive with a durable polyester-film release liner. This thin tape quickly builds a strong bond and is highly conductive in the Z-axis. It has excellent aging stability and offers important process, cost and performance advantages over mechanical, liquid and spray adhesive systems. Circle No. 159