Pressurex®, a thin, flexible film from Sensor Products Inc., is a versatile NDT tool for quality control and machine-component inspection. Its ability to easily and rapidly show inconsistencies in surface pressure between mating or contacting surfaces has lowered scrap rates and assisted in the design and manufacture of many industrial and electronic products.

Problem

Futek, a leading U.S. manufacturer and supplier of load cells, torque and pressure sensors, was having difficulty assembling some of its load cells to its specifications. By performing several tests and controlling for different variables, fluctuations in clamping pressure were found to be a significant factor.

Solution

Futek’s sensors incorporate metal foil strain gauge technology. The adhesive they use to bond the gauges to their sensors requires a clamping pressure of 50-75 psi. However, James Meiselbach, a Futek mechanical engineer, said that when they used Pressurex® film, pressure fluctuations of 50-200 psi or more in some production runs were revealed. This led Futek to use the film to help redesign several of their clamps to incorporate silicone die springs to more precisely regulate the pressure.

“A sample pack of Pressurex with film that revealed different surface-pressure ranges allowed our production to continue,” Meiselbach said.

The film reveals surface pressure of 2-43,200 psi (0.14-3,000 kg/cm2) and requires no training or instrumentation. It can assess surface contact inconsistencies in virtually any industrial or electronic application, including gaskets, clamps, bolted joints, connectors, heat sinks, heat-sealing elements, welding heads, and plastic and composite manufacture.

Meiselbach found using the Pressurex film to be a simple procedure. To measure the surface pressure of a clamp around the outside of a load cell, he cut the film to the configuration of the clamp surface area, placed it between the clamp and the load cell, applied force, unclamped it, and removed the film. He then compared the film, which changes color depending on how much pressure is exerted, to an accompanying color-calibration chart.

Meiselbach became aware of Pressurex while working for an aerospace company. “We were having a problem with the main rotor blade of a helicopter,” he said. “Interference was causing a fatigue crack in one of the inner spar tubes of the rotor blade. We put a large sheet of Pressurex in the bonding tool, bagged it up and pressurized it in the autoclave. When we removed the film, we were able to identify the exact amount of pressure causing the crack.”

About the Company

Established in 1990, New Jersey-based Sensor Products Inc. is a world leader in the manufacture and distribution of film and electronic tactile pressure-sensing solutions. The company  provides in-house and on-site stress- and pressure-mapping analysis, as well as consulting services and regional technical seminars.

For more information, phone (973) 884-1755 (USA), e-mail info@sensorprod.com or visit www.sensorprod.com.


Links

Did you enjoy this article? Click here to subscribe to Adhesives & Sealants Industry Magazine.

You must login or register in order to post a comment.

Multimedia

Videos

Podcasts

Environmentally Friendly Manufacturing

Edward Gotch, president of Emerald Kalama Chemical, talks about embracing sustainability with Susan Sutton, editor-in-chief.

More Podcasts

THE MAGAZINE

Adhesives & Sealants Industry Magazine

ASI May 2013 cover 100x133

2013 May

The 2013 May Adhesives and Sealants Industry Magazine includes articles about PPG and Bostik, as well as a Q&A about polyurethane. Check it out today!

Table Of Contents Subscribe

THE ADHESIVES STORE

handbook-sealant-tech.gif
Handbook of Sealant Technology

The Handbook of Sealant Technology provides an in-depth examination of sealants, reviewing their historical developments and fundamentals, adhesion theories and properties, and today’s wide range of applications.

More Products

asi1211p_Cover-DE.gifASI's Buyers' Guide

Annual purchasing resource for equipment used in the manufacture/formulation of adhesives, sealants, pressure sensitives, tapes and labels and for application of finished adhesives. 

Clear Seas Research

With access to over one million professionals and more than 60 industry-specific publications, Clear Seas Research offers relevant insights from those who know your industry best. Let us customize a market research solution that exceeds your marketing goals.

STAY CONNECTED

facebook_40px twitter_40  youtube_40pxlinkedin_40