Curing materials and equipment provider Dymax has been granted a patent for its HLC™ (Hybrid Light-Curable) adhesive platform. The new technology combines the optimal qualities of anionic polymerization and free radical chemistries into one formulation.
HLC technology aims to improve the curing performance of urethane (meth)acrylate compositions commonly used to formulate coatings, adhesives, sealants, and inks. The advantages of HLC include fast cure, low-to-no blooming after proper light cure, better aesthetics, humidity resistance, and more flexible joints than ordinary cyanoacrylates.
Exclusive Insights: Gain access to in-depth coverage of adhesive and sealant manufacturing, formulations and finished products. Comprehensive Coverage: Stay informed with the latest news and trends through our videos, podcasts, eNewsletters, webinars, continuing education resources, and a monthly eMagazine. Networking Opportunities: Connect with other industry professionals and leaders through our webinars and online platforms.