This high-strength adhesive is reportedly designed for industrial and laminating applications that require clarity, as well as excellent structural, mechanical, and electrical properties
TRA-BOND 2114 is a low-viscosity, transparent epoxy adhesive formulation. This high-strength adhesive is reportedly designed for industrial and laminating applications that require clarity, as well as excellent structural, mechanical, and electrical properties. It can be cured overnight at room temperature, or as quickly as four hours at 65ºC. Fully cured, it is a tough, durable and almost water-white electrical insulator that is resistant to water, gases and vapors, most petroleum products, salt solutions, mild acids, alkalis, and many other organic and inorganic compounds.