STYCAST 1495K encapsulant, cured with Catalyst 23, offers protection from temperature extremes found on the frames of automobiles, as well as road hazards such as water and salt. This material supports the electronics found in braking systems without compromising device integrity or reliability. This encapsulant is designed to protect stress-sensitive electronics from vibration and harsh operating environments. The product combines low coefficient of thermal expansion and Tg to survive thermal cycling from -40degC to 130degC. Circle No. 112